Abrasion Damage Factors For Material Handling ceramic lined elbow pipe

Material handling wear resistant ceramic elbow is the lifeblood of industrial production, to ensure the life of  pipeline is precondition of  safe and efficient production, compared with elbow pipe , abrasion damage of straight pipe is generally lower. Thus, the main consideration factor in pneumatic conveying is bend
chemshun ceramics - corrosion resistant
bend pipe liner for conveying powder

Tube wear damage. For example: the  handling material is strong abrasive materials such as iron, if  an ordinary steel elbow, Continuously convey materials for  two hours, the elbow will be worn; if the elbow bend radius is too small, brittle materials during transportation will have higher crushing rate

Our long-term lessons learned by the main factors that causing wear damage  as follows:

 (1)Physical properties of delivery  materials. Including the size and shape of the particles, concentration, hardness, moisture, broken rate and adhesion And so on.

(2) the status of the delivery tube. Metal materials and tissue components including pipelines, hardness, surface finish, the interior Diameter, shape and layout.

(3) transport conditions. Including conveying air velocity, feed gas ratio, temperature and flow status.

In the actual delivery, the influence of these factors on the wear and tear is not solely exist, but conbination of these Therefore, even if the same kind of material, using the same material conveying pipe, the abrasion damage degree is different because of different conveying conditions.
Chemshun ceramics mainly study abrasion damage problems with 92% 95% alumina ceramic linings welcome to  www.chemshun.com



MORE LINKS:


评论

此博客中的热门博文

What are the characteristics of abrasion-resistant ceramic tiles?

What are interlocking wear-resistant ceramic tile liner ?

How to improve the wear resistance of Al2O3 ceramics